Products FAQ

What is the difference between ABS AH36, DH36, EH36 and FH36?

ABS Grade AH36, DH36, EH36 and FH36 shipbuilding steel plates have the same strength; the key difference lies in the test temperature for low-temperature impact toughness.

GradeImpact Test TemperatureImpact Energy, KV2 / JSuitable for Marine Environments
ABS AH360°C34(Longitudinal), 24(Transverse)Standard marine environments.
ABS DH36-20°C34(Longitudinal), 24(Transverse)Cold-water marine environments.
ABS EH36-40°C34(Longitudinal), 24(Transverse)Polar marine environments with extremely low temperatures.
ABS FH36-60°C34(Longitudinal), 24(Transverse)Polar/ice regions and ultra-low-temperature deep-sea environments.

Customer Cooperation

Customers choose to engage in long-term cooperation with Yuxin Steel not only because of our high-quality products and services, as well as our strong reputation in the international market, but also due to our experienced one-stop raw material supply and further steel processing capabilities!

Wechat